Sub-10µm mSAP Processing: Ultra-High Density Interconnect (UHDI) Design Rules

MT

Marcus Thorne

Chief Process Engineer

Reviewed by: Advanced Lithography Group
UHDI Technology
Subtractive etching reaches its physical limit at 40µm line/space due to trapezoidal undercut. The Modified Semi-Additive Process (mSAP) leverages ultra-thin seed copper layers and electrolytic pattern plating to achieve vertical trace sidewalls down to 8µm/8µm, unlocking ultra-high density interconnects (UHDI).

1. Vertical Trace Profile vs. Subtractive Etch Factor

In traditional subtractive copper etching, chemical lateral etching creates sloped trapezoidal conductor profiles with an etch factor around 2.5 to 3.0, causing severe skin-effect impedance variations at gigahertz frequencies.

mSAP plates copper electrochemically inside photoresist trenches over an ultra-thin 2µm copper foil, achieving an etch factor exceeding 5.0 with near-vertical sidewalls (85°-90°), preserving design impedance targets.

Key Engineering Takeaways

  • Sub-10µm line and space enables 5x routing density improvement over standard HDI.
  • Vertical trace sidewalls eliminate impedance variance and high-frequency dispersion.

2. Laser Microvia Alignment and Target Pad Optimization

With trace pitches dropping below 20µm, conventional mechanically drilled vias and standard laser ablation capture pads (150µm) consume excessive board real estate.

Next-generation UV pico-second laser ablation achieves 25µm microvia holes on 50µm capture pads, backed by direct laser imaging (DLI) registration tolerances under ±8µm across 500x600mm panels.

Key Engineering Takeaways

  • UV pico-second lasers produce cleanly ablated 25µm vias without dielectric charring.
  • Direct laser imaging guarantees ±8µm layer-to-layer registration accuracy.

Subtractive HDI vs. mSAP UHDI Process Capabilities

Key physical constraints and tolerances comparing standard subtractive and mSAP fabrication.

Feature / DimensionStandard Subtractive HDIChipPCBA mSAP UHDIEngineering Notes
Minimum Line / Space (L/S)45µm / 45µm8µm / 8µmEnables sub-0.3mm pitch BGA escape routing
Laser Microvia Diameter75µm - 100µm25µm - 35µmStacked via-in-pad without resin voiding
Etch Factor (Sidewall Angle)2.5 (approx. 65°)> 5.0 (approx. 88°)Critical for controlled impedance repeatability
Tags:#UHDI#mSAP#Semi-Additive#Fine Line Pitch#Microvia
Fabrication Ready

Need Prototype for this Design?

Turn your high-speed schematics into reality with ChipPCBA. Automated DFM, fast turnaround from 24h, and IPC Class 2/3 inspection standard. Free DFM analysis with every instant quotation.

Related Engineering Articles

View all
Hardware Design8 min read

Glass Core Substrates for Next-Gen SiP & 2.5D/3D Semiconductor Packaging

Glass core substrates overcome the thermal expansion and warpage limits of organic substrates, delivering ultra-tight through-glass vias (TGV) and sub-micron dimensional stability for AI compute chiplets.

SMT Assembly9 min read

Ultra-Miniature 008004 Component SMT Assembly: Nano-Coated Stencil Design & Nitrogen Reflow Controls

Engineering rules for assembling 008004 (0201 metric) passives: aperture area ratios, Type 6 solder powder rheology, high-speed nozzle vision calibration, and nitrogen-inerted reflow.

SMT Assembly8 min read

Design for Assembly (DFA): Best Practices for 0.25mm Pitch BGA and 01005 Components

Essential solder paste aperture ratios, pad land patterns, solder mask dam clearances, and thermal relief design for 0.25mm Pitch BGA and ultra-fine pitch components.