3
Hardware DesignSiP & Packaging•Nov 18, 2026•8 min read

Glass Core Substrates for Next-Gen SiP & 2.5D/3D Semiconductor Packaging

DLC

Dr. Lin Chen

Principal Packaging Architect

Reviewed by: ChipPCBA Semiconductor Lab
SiP & Packaging
As semiconductor packaging scales to multi-reticle AI processors and high-density chiplets, traditional organic core materials suffer from warpage, coefficient of thermal expansion (CTE) mismatch, and dielectric loss. Glass core substrates provide near-zero warpage, high thermal tolerance, and ultra-high-density Through-Glass Vias (TGV) to enable the next paradigm of 2.5D and 3D heterogeneous integration.

1. Through-Glass Via (TGV) Pitch & Electrical Performance

Glass substrates feature an isotropic dielectric constant (Dk ~5.2) and ultra-low loss tangent (Df <0.003 at 50 GHz), making them vastly superior to standard BT resins and Ajinomoto Build-up Films (ABF) for high-speed serialized data channels.

Laser-induced deep etching (LIDE) enables TGVs with aspect ratios exceeding 10:1 and diameters down to 20µm at 50µm pitch, allowing high-density signal breakout without parasitic capacitive loading.

Key Engineering Takeaways

  • Through-glass via aspect ratios exceed 10:1 with sub-micron sidewall roughness.
  • Ultra-low dielectric loss ensures signal transmission integrity up to 100 GHz RF and optical modulation.

2. Thermal Expansion Matching and Silicon Die Coplanarity

A primary failure mechanism in large-area SiP assemblies (>70x70mm) is shear stress on micro-bumps caused by CTE mismatch between silicon (2.6 ppm/°C) and organic cores (12-16 ppm/°C).

Engineered borosilicate and aluminosilicate glass cores closely match silicon at 3.2-3.8 ppm/°C, virtually eliminating die-attach shear strain and enabling reliable flip-chip assembly of sub-40µm micro-bump arrays.

Key Engineering Takeaways

  • CTE matching (3.5 ppm/°C) reduces micro-bump shear stress by over 65%.
  • Near-zero panel warpage enables higher yield during SMT reflow and capillary underfill dispensing.

Glass Core Substrate vs. Organic ABF Benchmark

Comparative material and electrical parameters for high-density advanced packaging.

Parameter / MetricStandard Organic (ABF)Advanced Glass CoreEngineering Notes
Coefficient of Thermal Expansion (CTE)14 - 18 ppm/°C3.2 - 3.8 ppm/°C (Matched to Si)Drastically reduces solder fatigue in large dies
TGV / Microvia Aspect Ratio1:1 to 2:1 mechanically drilled> 10:1 laser-etched TGVSub-25µm diameter vias at 50µm pitch
Dielectric Loss (Df @ 28 GHz)0.012 - 0.018< 0.003Essential for 112G and 224G SerDes channels
Tags:#Glass Core Substrates#SiP#2.5D Packaging#Thermal Expansion#TGV
Fabrication Ready

Need Prototype for this Design?

Turn your high-speed schematics into reality with ChipPCBA. Automated DFM, fast turnaround from 24h, and IPC Class 2/3 inspection standard. Free DFM analysis with every instant quotation.

Related Engineering Articles

View all
News & Events5 min read

ChipPCBA Unveils SiP (System-in-Package) & 2.5D Substrate Quick-Turn Prototyping Capability

ChipPCBA commissions ultra-fine line 10µm/10µm semi-additive process (mSAP) lines and sub-50µm micro-bump flip-chip packaging for rapid SiP module turnaround.

Hardware Design12 min read

PCIe 6.0 & PAM4 High-Speed Design: 32+ Layer Stackup, Loss Budget & Surface Roughness Compensation

Comprehensive analysis of PAM4 4-level modulation loss budgets, Megtron 7 dielectric selection, copper foil roughness compensation, and backdrill stub resonance elimination for 64 GT/s channels.